Inquiries
inquiries@pokornyindustries.comAccess to prices and online shopping
Overview of your purchased items
Contact your sales representative and clerk
Educational materials
News about industrial seals
Information on new products and services
Exclusive hints and tips
Fill in your contact details and we will get back to you as soon as possible.
We will call you at your chosen time and advise you on what you need.
Our sales and technical representative will come to your company for a personal consultation.
Two black rubber materials look identical. One seals in oil for years, while the other swells and fails. A comparison of NBR, EPDM, FKM, and silicone—and the most common mix-ups.
Place NBR and EPDM sheets side by side: two identical black rubbers. One seals in oil for years; the other swells and fails. Mixing up rubber types is the most common material-selection mistake we see in industrial operations—and one table can help prevent it.
| Rubber | Temperature | Strengths | Weaknesses |
|---|---|---|---|
| NBR | −30 to 120 °C | mineral oils, greases, fuels | ozone, UV, steam |
| EPDM | −50 to 130 °C | hot water, steam, UV, weathering | mineral oils and greases |
| FKM/FPM (Viton®) | −20 to 200 °C | chemicals, oils, high temperatures | hot water/steam, price |
| VMQ (silicone) | −60 to 200 °C | wide temperature range, food use | abrasion, tear resistance |
| CR (neoprene) | −20 to 100 °C | weathering, refrigeration | limited range of applications |
| SBR | −30 to 100 °C | price, general-purpose use | oils, chemicals, ageing |
| NR (natural rubber) | −40 to 85 °C | elasticity, abrasion resistance | oils, ozone |
The values reflect our range of rubber rolls and sheets; check the product data sheet for the specific compound.
EPDM in oil – the rubber swells and softens, and the joint starts leaking. A typical scenario: “we replaced the seal with another one that was the same color.”
NBR in steam or outdoors – the rubber hardens and cracks. NBR has no place in sunlight or hot water.
Silicone in a dynamic application – low abrasion resistance means a short service life.
FKM in hot water – excellent chemical resistance does not mean resistance to steam.
Only reliably through laboratory testing. In practice, don’t try to identify it—specify it: buy rubber with a material data sheet and clear identification markings.
The same rules apply to O-rings, oil seals, and the elastomers used in mechanical seals. The wrong elastomer can cause even a correctly designed joint to fail. We can help you choose—including by checking the material against our chemical resistance database.
Get advice on material selection →
NBR resists oils and fuels, but not UV or steam. EPDM is exactly the opposite.
They refer to the same group of fluoroelastomers (trade name Viton®). FKM is used under ASTM, and FPM under ISO/DIN.
Silicone (VMQ) or certified-grade EPDM – see Food-grade seals.
You can’t tell them apart visually. Only laboratory testing is reliable—so always ask for a material data sheet.