O-Rings: Dimensions, Materials, and Error-Free Installation

How to read O-ring dimensions, choose a material, and why the groove determines the design. Four installation mistakes responsible for most leaks.

O-Rings: Dimensions, Materials, and Error-Free Installation

An O-ring is the simplest sealing element in the world—a piece of rubber with a circular cross-section that can seal hundreds of bar. That is, if four things are right: the size, the material, the groove and the installation. If an O-ring leaks, one of them is to blame.

How an O-ring seals

By compressing its cross-section in the groove. The deformed rubber fills the space, and the pressure of the fluid pushes it against the sealing surface—as pressure increases, the O-ring becomes self-energizing to a degree. The key factor is cross-section compression, typically 15–30% for static applications and 10–20% for dynamic ones.

Dimensions and designation

Two dimensions: inside diameter × cord cross-section (e.g. 25×3). Measure the groove and the components, not the old O-ring—the rubber will have taken a permanent set.

Watch out for standards: metric and inch series (AS568) differ. An O-ring from another series that is “almost the same” will not seal properly.

Material: the same rules apply as for any rubber

MaterialTemperatureApplications
NBR−30 to 120 °Coils, fuels – standard choice
EPDM−50 to 130 °Chot water, steam, outdoor environments
FKM−20 to 200 °Cchemicals, higher temperatures
VMQ (silicone)−60 to 200 °Cfood applications, extreme temperatures
PTFE / encapsulateddepending on designaggressive chemicals

Compare rubber types and learn about common mix-ups: NBR vs. EPDM vs. FKM. Check chemical resistance in our database.

The groove matters more than you might expect

Four installation mistakes behind most leaks

  1. Twisting the O-ring as it is fitted – causing spiral damage.
  2. Damage from an edge or thread – without an installation cone, any sharp edge can cut the O-ring.
  3. Dry installation – lubricate with the fluid or a compatible lubricant (mineral lubricant must not be used with EPDM).
  4. Stretching beyond the limit – the inside diameter can only tolerate a few percent of stretch.

Why O-rings age

Rubber under constant compression loses its elasticity (compression set): the O-ring takes the shape of the groove instead of retaining its circular shape, and can no longer compensate for changes in temperature and pressure. That is why O-rings should be replaced whenever an assembly is taken apart—a new one costs pennies, while a leak can mean downtime.


We supply O-rings in metric and inch series, with advice on groove design and material selection.

Request O-rings →

How do you measure an O-ring?

Inside diameter × cord cross-section (25×3 mm). Measure the groove, not the old, deformed O-ring.

How much compression should an O-ring have?

Typically 15–30% for static applications and 10–20% for dynamic ones – the exact value depends on the groove design and compound hardness.

Why does an O-ring leak immediately after replacement?

It may have been damaged during installation, be the wrong size due to a different standard series, or be made from a material unsuitable for the fluid.

When should you use backup rings?

At high pressures where there is a risk of the rubber being extruded into the clearance gap – typically in hydraulic applications.

Are you ready to put your seal selection worries behind you? Contact us

and get valuable advice and information on industrial seals